@article { author = {Narchin, Parvaneh and Saraeyan, Ahmad-Rezaa and afra, elyas}, title = {Improving the Antibacterial Effect of Pomegranate Peel Extract with Nano-chitosan Using Encapsulation Technique in Sanitary Papermaking}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {513-532}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {By developing attention to environmental issues and to the increasing attention of human society to health issues the use of environmentally friendly antibacterial compounds such as plant extracts for the production of antibacterial paper is very interesting. On the other hand, due to the high volatility of these environmentally friendly compounds, it is expected that encapsulating them in materials such as chitosan can increase their stability and control of release into the paper structure. Therefore, in this study, ethanolic extract of pomegranate peel in chitosan was encapsulated by ion gelation method and applied to the surface of the paper by spray method. The structural properties of pomegranate peel extract such as total phenol, total flavonoid and their antioxidant activity were investigated. Structural, barrier such as antibacterial activity and resistance properties of the prepared paper were also investigated. The results showed that nanocapsules of about 160 nm were obtained by ion gelation method, which were able to increase the antibacterial activity of the modified paper by about 35 mm against Staphylococcus aureus. In addition, the antibacterial activity of nanocapsule-modified paper was about two weeks higher than that of pure extract-modified paper. On the other hand, the presence of chitosan in the structure of nanocapsules also led to improved physical and resistance properties of the modified paper}, keywords = {Pomegranate Peel Extract,Nano- Chitosan,Chitosan- Pomegranate Peel Extract Nanocapsule,ionic gelation,Antibacterial Paper}, title_fa = {بهبود اثر ضد باکتری عصاره پوست انار با نانوکیتوزان با استفاده از روش انکپسوله کردن در ساخت کاغذهای بهداشتی}, abstract_fa = {با توسعه توجه به مسائل زیست‌محیطی و توجه هرچه بیشتر جامعه انسانی به مسائل بهداشتی استفاده از ترکیبات ضد باکتری دوستدار محیط‌زیست نظیر عصاره­های گیاهی برای تولید کاغذهای ضد باکتری بسیار جالب‌توجه می­باشد. از طرفی با توجه به فراریت بالای این ترکیبات دوستدار محیط‌زیست انتظار می­رود کپسوله کردن آن­ها در موادی نظیر کیتوزان بتواند موجب افزایش پایداری و کنترل رهایش آن­ها در ساختار کاغذ شود. ازاین‌رو در این تحقیق عصاره اتانولی پوست انار در کیتوزان به روش انعقاد یونی کپسوله شد و با استفاده از روش اسپری روی سطح کاغذها اعمال شد. ویژگی­های ساختاری عصاره پوست انار نظیر فنل کل، فلاونوئید کل و میزان فعالیت آنتی‌اکسیدانی آن­ها بررسی شدند. همچنین ویژگی­های ساختاری، ممانعتی نظیر فعالیت ضد باکتریایی و مقاومتی کاغذهای تهیه‌شده نیز موردبررسی قرار گرفتند. نتایج نشان دادند که با روش انعقاد یونی نانو کپسول‌هایی با ابعاد حدود 160 نانومتر به دست آمدند که توانستند فعالیت ضد باکتری کاغذهای اصلاح‌شده را حدود 35 میلی­متر در برابر باکتری استافیلوکوکوس اورئوس افزایش دهند. علاوه بر این فعالیت ضد باکتری کاغذهای اصلاح‌شده با نانو کپسول‌ها حدود دو هفته بیشتر از کاغذهای اصلاح‌شده با عصاره خالص بود. از طرف دیگر حضور کیتوزان در ساختار نانو کپسول‌ها نیز منجر شد تا ویژگی­های فیزیکی و مقاومتی کاغذهای اصلاح‌شده نیز بهبود یابند.}, keywords_fa = {عصاره پوست انار,نانوکیتوزان,نانو کپسول کیتوزان- عصاره پوست انار,انعقاد یونی,کاغذ ضد باکتری}, url = {https://www.ijwp.ir/article_38975.html}, eprint = {https://www.ijwp.ir/article_38975_5418959e49fe306904dfad1fdf208e93.pdf} } @article { author = {salehi, javad and Mirshokraee, Sayed Ahmmad and monfared, azam}, title = {Cellulose coating on Poly (Ethylene Terephthalate) yarn}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {533-541}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {Nowadays, Polyethylene terephthalate (PET) yarn are replaced by cotton yarn because they are cheaper than cotton yarn. However, some cellulose properties such as high Glass transition temperature (TG) and moisture absorption are among important features of cellulose that plastic yarn lacks. Molding and blending are usual techniques but decline mechanical properties. Therefore, in this research, the surface of artificial polymer was grafted with viscose and coated with cellulose. For PET coating in the first method, the surface of polymer was hydrolyzed by dipping in the H2SO4 85% solution, and then the product was grafted with cellulose by dipping in the viscose cellulose solution. In this method viscose cellulose was prepared with Ethylene diamine, and Cu (OH) 2.  In the second method, PET was first placed in a solution of H2SO4 85%, then was placed in a viscose cellulose solution that had been prepared by NaOH 50% and CS2. In the third method, the surface of polymer was hydrolyzed by NaOH solution and coated surface of polyester with paste of cellulose that included Ethylene glycol and urea. (FT-IR) were used to study properties of PET-graft-Cellulose fibers. The result of FT-IR exhibits coupling between PET and cellulose was accomplished and the first method is a better adhesive.}, keywords = {PET yarn,viscosecellulose,Coating Polymer}, title_fa = {پوشش سلولزی روی نخ پلی‌اتیلن ترفتالات}, abstract_fa = {امروزه نخ‌های، پلی‌اتیلن ترفتالات به دلیل ارزان بودن جایگزین نخ پنبه شده‌اند.  اما خواص سلولز مانند دمای انتقال شیشه (Tg) بالا و جذب رطوبت؛ ویژگی‌های مهمی است که نخ پلاستیکی ندارد. ذوب و مخلوط کردن پلی‌استر و سلولز روشی معمول است اما سبب کاهش مقاومت مکانیکی می‌شود.  بنابراین در این پژوهش سطح پلیمر مصنوعی پلی‌اتیلن ترفتالات با سلولز ویسکوز پیوند خورد و پوشش سلولزی برقرار شد. برای پوشش پلی‌اتیلن ترفتالات درروش اول, ابتدا سطح پلیمر در محلول H2SO4 85 درصد هیدرولیز شد سپس با قرار دادن در محلول سلولز ویسکوز؛ پلیمر با سلولز پیوند داده شد. در روش اول سلولز ویسکوز با اتیلن دی آمین و Cu(OH)2  تهیه شد. در روش دوم PET پس از قرار گرفتن در محلول H2SO4 85 درصد به مدت 5 دقیقه؛ داخل محلول سلولز ویسکوزی رفت که با استفاده از NaOH 50 درصد و CS2 تهیه‌شده بود. روش سوم هیدرولیز پلی‌اتیلن ترفتالات در محلول NaOH و پوشش آن با خمیر سلولزی که شامل آمیزه‌ای از اتیلن گلیکول و اوره بود. از طیف‌سنجی فروسرخ برای سنجش پیوند سلولز و PET استفاده شد. تفسیر نتایج FT-IR نشان داد پیوند شیمیایی بین PET و سلولز برقرارشده و در روش اول پیوند بهتری برقرارشده بود.}, keywords_fa = {نخ PET,سلولز ویسکوز,پوشش پلیمر,پاپ کاغذ}, url = {https://www.ijwp.ir/article_38980.html}, eprint = {https://www.ijwp.ir/article_38980_c29fcde00bc4fcc41cbe71357d157457.pdf} } @article { author = {asadpour, ghasem and boroshkian, hadi and Resalati, Hosain}, title = {Investigating the effect of refining on cellulase enzyme activity on the properties of OCC pulp}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {543-552}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {As the consumption of OCC pulp is increasing globally, practical studies are needed to reduce energy consumption and improve the quality of this pulp using enzymatic treatments. In this study, the effect of refining on cellulase enzyme performance on OCC pulp properties was investigated. OCC pulp with 4% consistency, 50 ° C constant temperature, 1 hour duration and 4-5.5: pH with cellulase enzyme at three levels of 0.1, 0.3, 0.5 percentages (based on dry weight of pulp) were pretreated. Pulp freeness and hand sheet strength properties were measured according to TAPPI standard codes. The results showed that the enzymatic treatment of cellulase increased pulp freeness and improved paper strength properties and this effect was more in unrefined OCC pulps than refined OCC pulps. Overall, enzymatic cellulase treatment can reduce pulp refining and reduce energy consumption and improve OCC pulp quality.}, keywords = {OCC pulp,cellulase enzyme,Mechanical properties,environment,Refining}, title_fa = {بررسی تأثیر پالایش در عملکرد آنزیم سلولاز بر خواص خمیر OCC}, abstract_fa = {از آنجا که  مصرف خمیر­کاغذ OCC  در دنیا در حال افزایش است، لازم است مطالعات کاربردی در خصوص کاهش مصرف انرژی و بهبود کیفیت این نوع خمیرکاغذ و با استفاده از تیمارهای آنزیمی انجام پذیرد. در این تحقیق تأثیر پالایش در عملکرد آنزیم سلولاز بر ویژگی­های خمیر­کاغذ OCC مورد بررسی قرار گرفت. خمیر­کاغذ OCC با درصد خشکی 4 درصد، در شرایط ثابت درجه حرارت 50 درجه­سانتیگراد، مدت زمان 1 ساعت و محدوده 5/4-4:pH با آنزیم سلولاز در سه سطح 1/0، 3/0، 5/0 درصد( بر اساس وزن خشک خمیر­کاغذ) پیش­تیمار شدند. درجه­روانی و ویژگی­های مقاومتی کاغذ بر اساس آئین­نامه­های استاندارد TAPPI  اندازه­گیری شد. نتایج نشان داد که تیمار آنزیمی سلولاز باعث افزایش درجه­روانی خمیر و بهبود ویژگی­های مقاومتی کاغذها شده و این تأثیر، در خمیر­های OCC پالایش­نشده بیشتر از خمیر­های OCC پالایش­شده ، بوده است. در مجموع با تیمار آنزیمی سلولاز می توان نسبت به کاهش پالایش خمیر و کاهش مصرف انرژی و بهبود کیفیت خمیر­کاغذ OCC اقدام نمود.}, keywords_fa = {خمیر کاغذ OCC,آنزیم سلولاز,ویژگی‌های مکانیکی,محیط زیست,پالایش}, url = {https://www.ijwp.ir/article_38991.html}, eprint = {https://www.ijwp.ir/article_38991_778c67a2a03bdaf1869871e3354f20e4.pdf} } @article { author = {sedaghat, akram and Oladi, Reza and Abdolkhani, Ali and Efhamisisi, Davood and Khandan Mirkohi, Azizollah and Mehramiz, Shayan}, title = {Effect of drought, fertilization, wounding and bending treatments on lignin content and composition of eucalyptus seedlings (Eucalyptus camaldulensis)}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {553-569}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In this study, the effects of drought, fertilization, wounding and bending treatments were investigated on the content and composition of wood lignin in two-year-old eucalyptus seedlings (Eucalyptus camaldulensis). Results showed that drought-induced xylem had the highest concentration of lignin and guaiacyl (G) units and the lowest amount of hydroxyphenyl (H) and syringyl (S) units as well as the lowest S/G ratio compared with other treatments. In contrast, the lowest concentration of lignin and G units and the highest amount of S units and the highest S/G ratio were observed in fertilization treatment. Due to this treatment, H units increased. After wounding, lignin concentration did not change significantly compared with the control treatment and only slightly decreased. However, as a result of this treatment, G units increased significantly and H and S units and S/G ratio decreased. The most important chemical change observed in bending treatment was a sharp increase in H units and a decrease in guaiacyl and syringyl and an increase in the S/G ratio. Overall, it can be concluded that the chemistry of xylem is altered to give the plant the best ability to withstand environmental stresses. Guaiacyl lignin has a more protective role, and increased H lignin is associated with increased growth rate or increased stem flexibility.}, keywords = {Lignin,Stress,xylem,Biochemistry}, title_fa = {تأثیر تیمارهای خشکی، کوددهی، زخم و خمش بر میزان و ترکیب لیگنین نهال‌های اکالیپتوس (Eucalyptus camaldulensis)}, abstract_fa = {در این پژوهش، تأثیر تیمارهای خشکی، کوددهی، زخم و خمش بر میزان و ترکیب لیگنین نهال‌های دوساله اکالیپتوس (Eucalyptus camaldulensis) موردبررسی قرار گرفت. نتایج نشان داد چوب پس از اعمال تیمار خشکی در مقایسه با سایر تیمارها، بیشترین غلظت لیگنین و واحدهای گواییاسیل (G) و کمترین مقدار واحدهای هیدروکسی‌فنل (H) و سیرینجیل (S) و همچنین کمترین نسبت S/G را دارد. برعکس، کمترین غلظت لیگنین و واحدهای G و بیشترین مقدار واحدهای S و بیشترین نسبت S/G در تیمار کوددهی دیده شد. در این تیمار، واحدهای H افزایش نشان دادند. در تیمار زخم در مقایسه با تیمار شاهد، غلظت لیگنین تغییر محسوسی نداشت و تنها به میزان ناچیزی کاهش یافت. با‌این‌حال براثر این تیمار، واحدهای G افزایش چشمگیری داشته و واحدهای H و S و نسبت S/G کاهش یافتند. مهم‌ترین تغییر شیمیایی دیده‌شده در تیمار خمش، افزایش شدید واحدهای H، کاهش لیگنین گواییاسیل و سیرینجیل و افزایش نسبت S/G بود. درمجموع، می‌توان نتیجه گرفت که شیمی بافت چوبی به‌گونه‌ای تغییر می‌یابد که به گیاه بهترین امکان مقابله با تنش‌های محیطی را بدهد. لیگنین گواییاسیل نقش حفاظتی بیشتری داشته و افزایش لیگنین H با افزایش سرعت رشد و یا افزایش انعطاف‌پذیری ساقه مرتبط است.   }, keywords_fa = {لیگنین,تنش,بافت چوبی,بیوشیمی}, url = {https://www.ijwp.ir/article_39034.html}, eprint = {https://www.ijwp.ir/article_39034_7364b66eeffc531956b12eca06c15bc4.pdf} } @article { author = {moezzipour, bita and moezzipour, aida}, title = {Investigation of using rice hask and paper waste to make free copper brake lining}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {571-583}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In this study, the properties of non-copper and non- asbestos friction materials were investigated using cellulose waste to make brake pads. Friction materials including 20% cellulose waste (rice husk and paper waste) were used to make industrial brake linings and the shear strength, wear rate and friction coefficient of the linings according to the relevant standards were tested. The results showed that the average of shear strength of brake pads made of rice husk in normal condition was 35% and after heating was 24% higher than the brake linings made of paper waste. Also, the average of friction coefficient of linings made of rice husk in the thermal stages of wear and friction test was 35% higher than that of the brake linings made of paper waste and the wear rate of linings made of rice paddy was 67% less than linings made of paper waste.  Also, all the properties of brake linings made of rice husk met the standard requirements. Thus, it can be said that by utilization of rice husk without copper and asbestos, the desirable properties of the brake pads can be achieved, and this formulation can be used in the production of automobile brake linings.}, keywords = {Cellulosic waste,Brake pads,Friction materials,Tribological Properties}, title_fa = {بررسی امکان استفاده از شلتوک برنج و پسماند کاغذ در ساخت لنت ترمز بدون مس}, abstract_fa = {در این پژوهش ویژگی­های مواد اصطکاکی بدون مس و آزبست، با استفاده از پسماند سلولزی برای ساخت لنت ترمز بررسی شد. مواد اصطکاکی حاوی 20 درصد پسماند سلولزی (شلتوک برنج و پسماند کاغذ) برای ساخت لنت ترمز به روش صنعتی مورداستفاده قرار گرفت و مقاومت برشی، نرخ سایش و ضریب اصطکاک نمونه­های لنت ساخته شده طبق استانداردهای مربوطه مورد آزمون قرار گرفت. نتایج نشان داد که میانگین مقاومت برشی لنت ترمزهای ساخته شده با شلتوک برنج در حالت نرمال، 35 درصد و پس از حرارت دادن، 24 درصد بیشتر از لنت ترمزهای ساخته شده با سلولز کاغذ است. همچنین میانگین ضریب اصطکاک لنت­های ساخته شده با شلتوک برنج در مراحل حرارتی آزمون سایش و اصطکاک، 35 درصد بیشتر از لنت ترمزهای ساخته شده با سلولز کاغذ و میانگین نرخ سایش لنت­های ساخته شده با شلتوک برنج، 67 درصد کمتر از لنت­های ساخته شده با سلولز کاغذ بود. هم­چنین کلیه ویژگی­های لنت ترمزهای ساخته شده با شلتوک برنج در حدود مجاز استاندارد بود؛ بنابراین می­توان گفت که لنت ترمز ساخته شده با استفاده از شلتوک برنج بدون مس و آزبست ویژگی­های مطلوبی دارد و می­توان از این فرمولاسیون در تولید لنت ترمز خودرو استفاده نمود.}, keywords_fa = {پسماند سلولزی,لنت ترمز,مواد اصطکاکی,ویژگی‌های سایشی}, url = {https://www.ijwp.ir/article_46147.html}, eprint = {https://www.ijwp.ir/article_46147_cee83cc42588b0c27193f03a9d89a21b.pdf} } @article { author = {Darvishi, Nasrin and Adeli, Kamran and Salmani, Unes}, title = {The Asymmetric Impacts of Currency Shocks on Wood Imports and Wood Products in Iran with Emphasis on the Environment of Shock Formation}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {585-598}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {Wood and wood products are used as a productive input as well as the final consumer goods of households. Part of this need comes from imports. Imports depend mostly on exchange rate developments, and importers respond differently to negative and positive currency shocks depending on currency conditions. Given the importance of this issue, the present study examines the asymmetric effects of foreign exchange shocks on wood imports and wood products in Iran, with an emphasis on the environment of foreign exchange shocks. In this regard, the EGARCH approach over the period 1974-2017 was used to model the formation of shocks and the data panel regression approach over the period 1993-2017 was used to investigate the asymmetric effects of shocks on wood imports and its products. The results show that the effect of negative and positive shocks on the amount of wood imports and its products is asymmetric. Trade openness reflects the ease of trade between Iran and its trading partners. The turbulent environment has reduced the impact of positive currency shock and increased negative impact of currency shock on the amount of raw wood imports, types of paper, and paper as final goods. The positive currency shock of the turbulent formation environment strengthens the effects of the exchange rate transition on the amount of finished goods and paper pulp. Positive and negative shocks have an asymmetric effect on the exchange rate environment. The effect of positive shocks is greater than negative shocks.}, keywords = {wood,Importation,Currency shocks,Asymmetric effects,EGARCH}, title_fa = {اثرات نامتقارن شوک‌های ارزی بر واردات چوب و فرآورده‌های چوبی در ایران با تأکید بر محیط شکل‌گیری شوک‌های ارزی}, abstract_fa = {چوب و فرآورده­های چوبی به‌عنوان نهاده­ تولیدی و همچنین کالای مصرفی نهایی خانوارها بکار گرفته می­شود. بخشی از این نیاز از طریق واردات تأمین می­شود. واردات بیش از هر چیزی به تحولات نرخ ارز بستگی دارد و واردکنندگان بسته به شرایط بازار ارز، به شوک­های منفی و مثبت ارز واکنش­های متفاوت نشان می­دهند. با توجه به اهمیت این مسئله، مطالعه­ی حاضر به بررسی اثرات نامتقارن شوک­های ارزی بر واردات چوب و فرآورده­های چوبی در ایران با تأکید بر محیط شکل­گیری شوک­های ارزی می­پردازد. در این راستا از رویکرد ایگارچ طی دوره­ی زمانی 1353 تا 1396 برای مدل‌سازی محیط شکل­گیری شوک­ها و از رویکرد رگرسیونی پانل دیتا طی دوره­ی زمانی 1372-1396 برای بررسی اثرات نامتقارن شوک­ها بر واردات چوب و فرآورده­های آن استفاده ‌شده است. نتایج نشان می­دهد که اثر شوک­های منفی و مثبت بر مقدار واردات چوب و فرآورده­های آن نامتقارن می­باشد. همچنین باز بودن تجاری نشان‌دهنده سهولت تجارت بین ایران و شرکای تجاری می‌باشد. محیط پرتلاطم باعث کاهش تأثیر شوک مثبت ارزی و افزایش تأثیر شوک منفی ارزی بر مقدار واردات چوب آلات خام، انواع کاغذ، کاغذ به‌صورت کالای نهایی شده است. شوک مثبت ارزی محیط شکل‌گیری پرتلاطم اثرات گذار نرخ ارز را بر مقدار واردات کالاهای نهایی و خمیرکاغذ تقویت می­کند. شوک مثبت و منفی بر محیط شکل‌گیری واریانس (تلاطم) نرخ ارز تأثیر نامتقارن دارد. اثر شوک­های مثبت بیشتر از شوک­های منفی هست.}, keywords_fa = {چوب,واردات,شوک‌های ارزی,اثرات نامتقارن,رویکرد ایگارچ}, url = {https://www.ijwp.ir/article_39048.html}, eprint = {https://www.ijwp.ir/article_39048_4c307291414b72e35072d780723baff9.pdf} } @article { author = {رسولی, داود and Asadian, Monireh and Rafighi, Ali and Khazaian, Abolghasem}, title = {Study on physical properties and weathering resistance of wood modified by formaldehyde-based resins containing nano zinc oxide}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {599-610}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {The use of wood in outdoor applications causes problems such as dimensional change, weathering and biological degradation. In this study, poplar wood was modified by three types of amino resins (melamine, melamine-urea and urea formaldehyde resins) and nano Zinc oxide (0, 0.5 wt%). Then, the physical properties and weathering resistance of modified wood after six months natural weathering were measured. The results showed that the treatment of wood with amino resins reduced water absorption and improved dimensional stability of samples in which melamine formaldehyde resin had the best performance. Moreover, the addition of nano zinc oxide to the amino resins enhanced their performance in improving dimensional stability of samples. The results of the colorimetry and microscopic images indicate that the treating by melamine formaldehyde reduced the color changes and surface morphology of the samples, although the use of nano zinc oxide did not have a positive effect in this regard.}, keywords = {Poplar wood,Formaldehyde-based resins,nano zinc oxide,Natural weathering}, title_fa = {بررسی خصوصیات فیزیکی و مقاومت به هوازدگی چوب اصلاح شده با رزین های بر پایه فرمالدئید حاوی نانواکسید روی}, abstract_fa = {ازآنجایی‌که استفاده از چوب در محیط­های بیرونی سبب بروز مشکلاتی از قبیل تغییر ابعاد، هوازدگی و تخریب بیولوژیکی می­شود، تصمیم گرفته­ شد تا در این پژوهش ساختار چوب صنوبر دلتوئیدس با استفاده از سه نوع رزین ملامین فرمالدئید (MF)،‌ ملامین­-اوره فرمالدئید (MUF) و اوره فرمالدئید (UF) به همراه (0 و 5/0 درصد) نانواکسید­روی اصلاح گردد سپس خصوصیات فیزیکی و مقاومت به هوازدگی نمونه­ها بعد از شش ماه هوازدگی طبیعی موردمطالعه قرار گرفت. نتایج به‌دست‌آمده نشان داد که تیمار چوب با رزین‌های آمینی موجب کاهش جذب آب و بهبود ثبات ابعادی شده است. رزین ملامین فرمالدئید بهترین عملکرد را در ارتباط با این ویژگی‌ها داشت. همچنین حضور نانو اکسید روی در ساختار رزین­ها موجب تقویت عملکرد آن‌ها در بهبود ثبات ابعادی نمونه­ها شد. نتایج حاصل از رنگ­سنجی و تصاویر استریو میکروسکوپی نشان داد که تیمار با رزین ملامین فرمالدئید باعث کاهش تغییرات رنگی و مرفولوژی سطح شده است. استفاده از نانو اکسید روی تأثیر مثبتی در این زمینه از خود نشان نداد.}, keywords_fa = {چوب صنوبر,رزین‌های بر پایه فرمالدئید,نانو اکسید روی,هوازدگی طبیعی}, url = {https://www.ijwp.ir/article_39908.html}, eprint = {https://www.ijwp.ir/article_39908_d37345e986dfd12feb85fa779bdb041f.pdf} } @article { author = {akhtari, maliheh and Arefkhani, Mehdi and azizi, majid}, title = {Determination of Concentration Level and Market Analysis of Iran Particle Board Imports}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {611-626}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {The importance of market concentration for government decisions and policies to regulate the market is inevitable. In this study, market indexes were calculated to identify the market status of particleboard imports and to help industry practitioners to identify the particleboard market and identify production potential. In this study, the market structure was measured using concentration ratios, Herfindahl-Hirschman, Hall Tideman, Comprehensive Industrial Concentration, and Hannah-Kay. The market structure was measured for the period 2010-2019. According to the calculations, the average concentration ratio of the four major exporting countries to Iran for the ten-year period studied was 97.81% of the total import of particle board to the country. They indicates a market with a multilateral monopoly. Other indicators include the Herfindahl-Hirschman index at 5,561, the Hall Tideman index at 0.54, the Comprehensive Industrial Concentration Index at 0.79, and the Hall Tideman Index at α value of 0.6 to 3.12, α value was equal to 1.5, to 2.27 and α value was equal to 2.5 to 2.02. The results have shown that the market situation on the import of paticle board was the multilateral monopoly. The status of this monopoly has fluctuated and changed over the past ten years due to the political and economic decisions of governments and the change in domestic production of particleboard. In this market situation, exporting countries can argue over price and export rates. Turkey, United Arab Emirates, Thailand, Italy and Russia has been Iran's most important trading partner in the particleboard import market during the period under review, with the most imports being indexed to these countries, indicating a multilateral monopoly.}, keywords = {Concentration ratios,Herfindahl-Hirschman,Hall Tideman,Comprehensive Industrial Concentration,and Hannah-Kay and particleboard}, title_fa = {تعیین میزان تمرکز و تحلیل بازار واردات تخته خرده‌چوب ایران}, abstract_fa = {اهمیت تمرکز بازار جهت اخذ تصمیمات و سیاست‌های دولت در جهت تنظیم بازار امری اجتناب‌ناپذیر است. در این تحقیق به منظور شناخت وضعیت بازار واردات تخته خرده‌چوب شاخص‌های بازار محاسبه گردید تا به دست‌اندرکاران و دولتمردان این صنعت جهت شناخت بازار تخته‌خرده‌چوب و شناسایی پتانسیل تولید کمک نماید. با استفاده از شاخص‌های نسبت تمرکز، هرفیندال– هیرشمن، هال- تایدمن، جامع تمرکز صنعتی و هانا-کای، ساختار بازار برای بازه‌ زمانی سال‌های 1388 لغایت 1397 تحلیل شد. طبق محاسبات انجام شده میانگین شاخص نسبت تمرکز چهار کشور عمده صادر کننده به ایران برای دوره ده ساله مورد مطالعه به میزان 81/97 درصد از کل واردات تخته خرده چوب به کشور بوده است که نشان‌دهنده یک بازار با انحصار چندجانبه می باشد. دیگر شاخص‌ها نیز شامل شاخص هرفیندال– هیرشمن به مقدار 5561، شاخص هال تایدمن به مقدار 54/0، شاخص جامع تمرکز صنعتی به میزان 79/0 و شاخص هال تایدمن در مقادیر α برابر با 6/0به میزان 12/3، در α برابر با 5/1 برابر با 27/2 و در مقدار α برابر با 5/2 به میزان 02/2 بوده است. در نهایت نتایج گویای وضعیت بازار انحصار چند جانبه واردات تخته خرده چوب بوده است. وضعیت این انحصار با توجه به تصمیمات سیاسی و اقتصادی دولت ها و تغییر و تحول در تولید داخلی تخته خرده‌چوب در دوره ده‌ساله نوسان داشته و میزان انحصار تغییر نموده است ولی در کل، بازار واردات تخته خرده‌چوب از بازارهای انحصاری در ایران بوده و در این وضعیت بازار، کشورهای صادرکننده می توانند بر سر قیمت و میزان صادرات با یکدیگر اعتلاف نمایند. ترکیه، امارات، تایلند، ایتالیا و روسیه طی دوره مورد بررسی از مهم‌ترین شرکای تجاری ایران در بازار واردات تخته خرده‌چوب بوده‌اند به طوری که براساس شاخص‌ها بیشترین واردات از این کشورها بوده و نشان‌دهنده‌ی انحصار چند جانبه حاکم بر این بازار می‌باشد. }, keywords_fa = {شاخص‌های نسبت تمرکز,هرفیندال– هیرشمن,هال تایدمن,جامع تمرکز صنعتی و هانا-کی,تخته خرده‌چوب}, url = {https://www.ijwp.ir/article_39909.html}, eprint = {https://www.ijwp.ir/article_39909_f1bf656eee2e936848f0a382385db837.pdf} } @article { author = {Mousavi, Seyedeh Faegheh and Rezayati Charani, Pejman and Moradian, Mohammad Hadi and asadpour, ghasem}, title = {Improvement of wet and dry layer strengths of paper from chemi-mechanical pulp using polyamide epichlorohydrin and cellulose nanofibers vs imported long fiber Kraft pulp}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {627-643}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {The wet layer tensile strengths of the paper during production affects the frequency of breaking and its runability in the papermachine. In this study, the possibility of using cellulose nanofibers (NFC) and polyamide epichlorohydrin (PAE) vs imported long fiber  kraft pulp (LF) was investigated to improve the wet  and dry layer strengths of handsheet papers made from chemi-mechanical pulp (CMP). Strength properties of never-dried wet layer of papers with 35% consistency and air-dried papers were evaluated by pulp suspention and addition of 0 and 20% mineral calcium carbonate, NFC (at 2 levels, 2% and 3%), PAE (at 3 levels, 0.5%, 0.7% and 1%) and 20% of LF. Also, the effect of thermal treatments on the wet layer  strength of papers containing 3% NFC and 0.7% PAE at 100 and 130 °C tempratures was evaluated. Results showed that the addition of NFC together with PAE improves the wet and dry  layer strength properties of  papers. In the case of wet layers of  papers with 35% consistency, the addition of 3% NFC together with 1% PAE increased the tensile absorption energy (TEA) to 85%, although this was not as effective as using 20% LF (117%). In the case of air-dried papers, addition of 3% NFC and 1% PAE improved the papers TEA and tensile strength by 35% and 18%, respectively compairing with the addition of 20% LF. As a result of thermal treatments at 100 and 130 °C, the tensile strength of dried papers increased to 22 and 22.5%, respectively compared with the non-thermal treated papers. Overall, due to the positive performance of using NFC and PAE with thermal treatments, the combined use of 3% NFC and 1% PAE in CMP can be replaced by 15% LF to improve wet and dry papers strengths.}, keywords = {Tensile energy absorption (TEA),Wet and Dry paper strength,Polyamide epichlorohydrin (PAE),Nanofibrillated Cellulose (NFC),Chemi-Mechanical Pulp (CMP)}, title_fa = {بهبود مقاومت لایه تر و خشک کاغذ حاصل از خمیرکاغذ شیمیایی- مکانیکی با استفاده از پلی‌آمید اپی‌کلروهیدرین و نانوالیاف سلولزی در مقایسه با خمیرکاغذ کرافت الیاف بلند وارداتی}, abstract_fa = {مقاومت کششی لایه‌تر کاغذ هنگام تولید در تناوب پارگی و قابلیت حرکت آن در ماشین کاغذ تأثیر دارد. در این پژوهش، امکان استفاده از نانوالیاف سلولزی (NFC) و پلی­آمیداپی‌کلروهیدرین (PAE) در مقایسه با خمیرکاغذ کرافت الیاف بلند وارداتی (LF) برای بهبود خواص استحکامی لایه‌تر و ورق خشک کاغذ­های دست­ساز حاصل از خمیرکاغذ شیمیایی- مکانیکی (CMP) مورد بررسی قرار گرفت. خواص استحکامی لایه‌تر کاغذهای هرگز خشک نشده با 35 درصد خشکی و کاغذهای هوا - خشک، از طریق آماده­سازی سوسپانسیون خمیرکاغذ با افزودن 0 و 20 درصد کربنات کلسیم رسوبی، NFC (در 2 سطح 2 و 3 درصد)، PAE (در 3 سطح 5/0، 7/0 و 1 درصد) و 20 درصد LF مورد ارزیابی قرار گرفت. همچنین اثر تیمارهای حرارتی بر لایه‌تر کاغذهای حاوی 3 درصد NFC و 7/0 درصد  PAE در دماهای 100 و 130 درجه سلسیوس مورد بررسی قرار گرفت. نتایج نشان داد افزودن NFC همراه PAE باعث بهبود در ویژگی­های استحکامی لایه‌تر و ورق خشک کاغذها می­شود. در مورد لایه‌تر کاغذهای با 35 درصد خشکی، تیمار مربوط به افزودن 3 درصد NFC همراه 1 درصد PAE انرژی جذب کششی (TEA) را 85 درصد افزایش داد اگرچه این مقدار در حد تأثیر استفاده از 20 درصد LF نبود (117 درصد). در مورد کاغذهای هوا خشک، تیمار مربوط به افزودن 3 درصد NFC  و 1 درصد PAE انرژی جذب کششی و مقاومت کششی کاغذ را در مقایسه با تیمار 20 درصد LF به ترتیب 35 درصد و 18 درصد بیشتر بهبود داد. در اثر تیمارهای حرارتی کاغذهای حاصل از خمیرکاغذ حاوی 3 درصد NFC و 7/0 درصد PAE، مقاومت کششی کاغذهای خشک شده در دماهای 100 و 130 درجه سلسیوس نسبت به کاغذ بدون تیمار حرارتی به ترتیب 22 و 5/22 درصد افزایش یافت. به‌طورکلی با توجه به افزایش عملکرد مثبت استفاده از NFC به همراه PAE با اعمال تیمارهای حرارتی، استفاده توأم از 3 درصد NFC و 1 درصد PAE با خمیرکاغذCMP، قابلیت جایگزینی با 15 درصد LF برای بهبود مقاومت لایه‌تر و ورق خشک کاغذ حاصل از خمیرکاغذ شیمایی- مکانیکی را می­تواند داشته باشد.}, keywords_fa = {انرژی جذب کششی(TEA),استحکام‌ لایه تر و خشک کاغذ,خمیرکاغذ شیمیایی- مکانیکی(CMP),پلی‌آمیداپی‌کلروهیدرین(PAE),نانوالیاف سلولزی(NFC)}, url = {https://www.ijwp.ir/article_40496.html}, eprint = {https://www.ijwp.ir/article_40496_eaa190fd3ab3e4bdc7a4c656b29b5764.pdf} } @article { author = {قربانی, مریم and Asghari Aghmashhadi, Zahra and Amininasab, seyyed Mojtaba and Abedini, Raoufeh}, title = {The effect of different modification conditions on the efficiency of poplar wood epoxidation and the physical properties of the product}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {645-656}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {Wood modification with epoxy compounds, such as glycidyl methacrylate, could result in less moisture absorption and dimensional changes due to reduction in the number of hydroxyl groups and cell wall bulking. It is likely that change in the conditions of modification reaction would have a favorable effect on the physical properties by increasing the hydroxyl group’s substitution. To determine the optimal modification condition with glycidyl methacrylate, samples were modified at different concentrations (10, 20 and 30%), temperatures (90, 120 and 150°C) and times (8, 16 and 24 hours). Based on spectrum analysis, decrease of hydroxyl groups intensity and increase of carbonyl groups intensity confirmed cell wall modification with glycidyl methacrylate. Cell wall bulking and hydrophobing due to modification led to a reduction in porosity and free water adsorption. According to the results of soaking-drying cyclic test, increase of glycidyl methacrylate concentration led to the reaction with more number of hydroxyl groups, and higher temperature and longer duration of modification reaction also led to an increase in the reactivity of the epoxy groups with the wood cell wall. The higher temperature of reaction led to maintenance of weight gain due to modification, via formation of a more stable structure against hydrolysis. Scanning electron microscopic images confirmed cell wall swelling and polymerization of glycidyl methacrylate in wood cavities. In a general conclusion, it can be claimed that the concentration of 20%, the temperature of 150°C and the time of 16 hours are the optimal conditions for modification with glycidyl methacrylate.}, keywords = {glycidyl methacrylate,epoxide,Fourier transform infrared spectroscopy (FTIR),physical properties,Scanning microscopic images}, title_fa = {اثر شرایط مختلف اصلاح بر کارایی اپوکسیددار کردن چوب صنوبر و خواص فیزیکی فرآورده}, abstract_fa = {اصلاح چوب با ترکیبات اپوکسید مانند گلیسیدیل­متاکریلات می­تواند با کاهش تعداد گروه­های هیدروکسیل و حجیم­کنندگی دیواره سلولی، به کاهش جذب رطوبت و تغییرات ابعاد چوب بیانجامد. این احتمال وجود دارد که تغییر شرایط واکنش اصلاح، با بهبود جانشینی گروه­های هیدروکسیل دیواره­های سلولی چوب، اثر مطلوب­تری بر خواص فیزیکی چوب داشته­باشد. برای تعیین شرایط بهینه اصلاح با ترکیب گلیسیدیل­متاکریلات، نمونه­ها در سطوح مختلف غلظت (10، 20 و 30 درصد)، دما (90، 120 و 150 درجه سانتی‌گراد) و زمان (8، 16 و 24 ساعت) اصلاح شدند. بر اساس تجزیه‌ و تحلیل طیف­ها، کاهش شدت گروه­های هیدروکسیل و افزایش شدت گروه­های کربونیل نشان­دهنده اصلاح دیواره سلولی با ترکیب اپوکسید می­باشد. حجیم­شدگی و آب­گریز شدن دیواره طی اصلاح با ترکیب اپوکسی، به کاهش تخلخل و جذب آب آزاد منتهی شد.­ بر اساس نتایج آزمون دوره­ای غوطه­وری- خشک‌کردن، افزایش غلظت گلیسیدیل­متاکریلات به واکنش تعداد بیشتری گروه اپوکسی با گروه هیدروکسیل و دمای بالاتر و زمان طولانی­تر نیز به افزایش واکنش­پذیری گروه­های اپوکسی با دیواره سلولی چوب منتهی شد. دمای بالاتر واکنش با تشکیل ساختار پایدارتر در برابر هیدرولیز، به حفظ بیشتر افزایش وزن ناشی از اصلاح منتهی شد. تصاویر میکروسکوپ الکترونی، واکشیدگی دیواره سلولی و پلیمر شدن گلیسیدیل متاکریلات در حفرات چوب را تائید می­نماید. در یک نتیجه­گیری کلی می­توان اظهار داشت که غلظت 20 درصد، دمای 150 درجه سانتی‌گراد و زمان 16 ساعت به­عنوان شرایط بهینه اصلاح با گلیسیدیل­متاکریلات تعیین شد.}, keywords_fa = {گلیسیدیل‌متاکریلات,اپوکسید,طیف‌سنجی مادون قرمز‌تبدیل‌فوریه,خواص فیزیکی,تصاویر میکروسکوپ الکترونی}, url = {https://www.ijwp.ir/article_40588.html}, eprint = {https://www.ijwp.ir/article_40588_1b195a75793a61814179afc441543ddf.pdf} } @article { author = {Jarzadeh, Borhan and قربانی, مریم and Dastoorian, forogh and amini nasab, seyyed mojtaba}, title = {Determination the optimal condition for surface modification of spruce wood with Rosin Maleic}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {657-668}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {Surface modification with natural modifiers containing chemical bonding agents including rosin maleic can improve the physical properties of wood by reducing the number of hydroxyl groups. It is likely that an increase of temperature or the presence of a catalyst will have a more desirable effect on the physical properties of the wood by improving the hydroxyl group’s substitution of the wood cell wall. This study was conducted to investigate the effect of different temperature levels and the presence of aluminum chloride catalyst for applying surface modification with Rosin Maleic, and evaluating the efficiency of the modification on the physical properties of Spruce wood. The samples were immersed in a rosin maleic solution with a concentration of 40% by weight/ volume (in toluene/xylene solvent) for 24 hours, and were heated for determine the effect of temperature, catalyst and leaching, under two temperature levels of 60°C, with and without catalyst, and 140°C, for 4 hours. According to the results, modification by reducing the hydroxyl groups (based on the infrared spectrums), improved hydrophobicity and dimensional stability of the treated samples. At the end of water immersion period, the higher temperature of reaction with formation a more stable structure against hydrolysis, led to maintenance the weight percent gain of modification. Increasing the modification reaction temperature from 60°C to 140°C create a significant difference in the measured properties, but the presence of the catalyst in the modification at 60°C reduced this difference and formed more stable structures. In a general conclusion, it can be claimed that the use of aluminum chloride as a catalyst in modification with rosin maleic, makes possible applying surface modification at ambient temperature, by forming a more stable structure against hydrolysis.}, keywords = {Surface modification,rosin maleic,Aluminum chloride,Fourier transform infrared spectroscopy (FTIR),physical properties,Contact angle}, title_fa = {تعیین شرایط بهینه اصلاح سطحی چوب نوئل با روزین‌مالئیک}, abstract_fa = {اصلاح سطحی با ترکیبات اصلاح‌کننده طبیعی دارای عامل اتصال شیمیایی مانند روزین­مالئیک می­تواند با کاهش تعداد گروه­های هیدروکسیل، به بهبود خواص فیزیکی چوب منتهی­شود. این احتمال وجود دارد که افزایش دما یا حضور کاتالیزور، با بهبود جانشینی گروه­های هیدروکسیل دیواره سلولی چوب، اثر مطلوب­تری بر فرآیند واکنش و خواص فیزیکی چوب داشته­باشد. تحقیق حاضر با هدف بررسی اثر سطوح مختلف دما و حضور کاتالیزور کلریدآلومینیوم برای اعمال اصلاح سطحی با روزین­مالئیک و ارزیابی کارایی این اصلاح بر خواص فیزیکی چوب نوئل انجام شد. نمونه­ها به مدت 24 ساعت در محلول روزین­مالئیک به غلظت 40 درصد وزنی/حجمی (در حلال تولوئن/ زایلن) غوطه­ور شدند. گرمادهی نمونه­ها، برای تعیین اثر دما، کاتالیزور و آبشویی کوتاه­مدت، تحت دو سطح دمایی 60 درجه سانتی­گراد، با و بدون کاتالیزور نمکی و 140 درجه سانتی‌گراد، در زمان 4 ساعت اعمال گشت. بر اساس نتایج طیف­سنجی مادون­قرمز تبدیل فوریه، اعمال اصلاح با کاهش گروه­های هیدروکسیل موجب بهبود آب‌گریزی و ثبات ابعاد نمونه­های تیمارشده گردید. در خاتمه بازه غوطه­وری در آب، دمای بالاتر واکنش با تشکیل ساختار پایدارتر در برابر هیدرولیز، به حفظ افزایش­وزن ناشی از تیمار منتهی گردید. افزایش دمای واکنش اصلاح از 60 به 140 درجه سانتی‌گراد، تفاوت معنی­داری در صفات اندازه­گیری شده ایجاد کرد، ولیکن حضور کاتالیزور در اصلاح تحت دمای 60 درجه سانتی‌گراد، به تشکیل ساختارهای پایدارتر منتهی شد. در یک نتیجه­گیری کلی می­توان اظهار داشت که بکارگیری کاتالیزور نمکی کلرید آلومینیوم در واکنش تیمار با روزین­مالئیک، با تشکیل ساختار پایدارتر در برابر هیدرولیز، امکان اعمال اصلاح سطحی در دمای محیط را میسر می­سازد.}, keywords_fa = {اصلاح سطحی,روزین‌مالئیک,کلریدآلومینیوم,طیف‌سنجی مادون قرمز‌تبدیل‌فوریه,خواص فیزیکی,زاویه تماس}, url = {https://www.ijwp.ir/article_40610.html}, eprint = {https://www.ijwp.ir/article_40610_86048c9b4ef8b243925dcb3e222e1bdf.pdf} } @article { author = {Ataefar, Ahmad and Zarea Hosseinabadi, Hamid and Afshar Taremi, Faramarz and azizi, majid}, title = {Effect of Blending Butylacrylate with Unsaturated Polyester Resin on Toughness of Matrix and Mechanical Properties of Kenaf and Glass Fiber- based Composites}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {669-682}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {In this study, the effect of blending butyl acrylate with orthophthalic unsaturated polyester resin were investigated on toughness of the matrix and some mechanical properties of the composites with the same matrix. In the first phase, the blends, as matrix, have been fabricated by two different curing systems (cold cure with methyl ethyl ketone peroxide as catalyst, and hot cure with di-benzoyl peroxide as catalyst), each by combinations of 0, 5, 10, 15, 20 and 25 % monomeric butyl acrylate. Izod impact test was used to evaluate the toughness of blended matrix and pure matrix. In the second phase, kenaf and glass fiber-based composites were made by the blended matrix with the highest impact strength, then subjected to some mechanical tests such as toughness, failure energy, ultimate strength, modulus of elasticity, and heat deflection temperature. Test results showed that the highest value for impact strength, as 1.91 kJ m-2 was attained for cold curing system with 15% monomeric butyl acrylate. Impact strength or toughness of blended matrix/fiber composites was around 31% more than that of for pure polyester/fiber composites. In addition, modulus of elasticity of blended matrix reinforced by fibers was around 133% less than that of for pure polyester/fiber composites. Finally, the results showed that monomeric butyl acrylate had a negative effect on ultimate strength and heat deflection temperature of blended matrix/kenaf and glass fiber-based composites}, keywords = {unsaturated polyester,monomeric butyl acrylate,glass fiber based composite,kenaf fiber based composite,Mechanical properties}, title_fa = {تاثیرآلیاژسازی رزین پلی استر غیراشباع با بوتیل اکریلات برچقرمگی ماتریس و خواص مکانیکی کامپوزیت الیاف کنف و شیشه}, abstract_fa = {در این تحقیق اثر آمیختگی رزین پلی­استرغیراشباع­ارتوفتالیک با مونومر بوتیل­اکریلات بر چقرمگی این آلیاژ و همچنین کامپوزیت ساخته ­شده با آن بررسی‌شده است. در فاز اول، آلیاژ مورد نظر با دو شرایط متفاوت و هر کدام با ترکیب درصدهای 0، 5، 10، 15، 20 و 25 درصد بوتیل­اکریلات پخت و آماده سازی شده است. پخت سرد با کاتالیست متیل­ا­تیل­­­کتون ­پراکسید و پخت گرم با کاتالیست دی­بنزوئیل­پراکسید. از آزمون مقاومت به ضربه ایزود برای ارزیابی میزان چقرمگی نمونه­های آلیاژ شده استفاده شد. در فاز دوم، از آلیاژ با بالاترین میزان چقرمگی به عنوان ماتریس برای ساخت کامپوزیت­های الیاف­کنف و الیاف­شیشه استفاده شد و خواص مکانیکی آن­ها شامل چقرمگی، انرژی شکست، استحکام در نقطه شکست، مدول الاستیسیته و دمای انحنای حرارتی مورد ارزیابی قرار گرفت. نتایج نشان داد بیشترین چقرمگی ماتریس مربوط به سطح 15­درصد بوتیل­اکریلات در سیستم پخت سرد برابر با 91/1 kJ/m2 می‌باشد. در مقایسه با کامپوزیت با ماتریس پلی­استر­خالص، چقرمگی در کامپوزیت با ماتریس آلیاژ پلی­استر به میزان حدود 31 درصد افزایش داشته است. نتایج مدول­الاستیسیته کامپوزیت­ها نشان داد مدول­الاستیسیته کامپوزیت با ماتریس آلیاژ شده با بوتیل اکریلات حدود 133 درصد کمتر از مقدار این ویژگی برای کامپوزیت با ماتریس پلی استر خالص می‌باشد. همچنین مشخص شد استفاده از مونومر بوتیل­اکریلات باعث کاهش استحکام در نقطه شکست و دمای انحنای حرارتی کامپوزیت های الیاف شیشه و کنف با ماتریس آلیاژ شده، گردیده است.}, keywords_fa = {پلی‌استرغیراشباع ارتوفتالیک,مونومربوتیل اکریلات,آلیاژ کردن,کامپوزیت الیاف شیشه,کامپوزیت الیاف کنف,چقرمگی,مدول الاستیسیته}, url = {https://www.ijwp.ir/article_46150.html}, eprint = {https://www.ijwp.ir/article_46150_d57ef35aa24a1e5b9fdd9b8b4161c8ef.pdf} } @article { author = {دادمحمدی, کبری and mohamadi achacheloei, mohsen and jafrai, mohamad taghi}, title = {Influence of the cellulose nanofibers on optical and mechanical strength of the historical paper relics}, journal = {Iranian Journal of Wood and Paper Industries}, volume = {11}, number = {4}, pages = {683-692}, year = {2021}, publisher = {Iranian Scientific Association of Wood and Paper Industries}, issn = {2008-9066}, eissn = {2423-3242}, doi = {}, abstract = {The purpose of this study was to evaluate the effect of cellulose nanofibers and its use as a strength enhancer to restore tensile strength and durability to historical paper relics. This research was conducted by analytical comparisons method and samples were collected by experiments related to research topics such as pH measurement, calorimetric and the measurement of tensile strength of the samples. In this study, treatment of cellulose nanofibers with weight percentages of 0.5, 1 and 2%, was prepared as a suspension with water and used to consolidation of the paper samples. The treatment was sprayed three times by 3.5 ml using spray can, then the treatment samples were thermally aged for 144 h at D776-92 ASTM, at a temperature of 105 °C. Next, changes of pH, color and tensile strength of the specimens were investigated. Results showed that the pH of the samples after treatment ranged from 6.98 to 7.17 and after the aging, pH of the samples was in the near alkaline range of 6.85 to 7.11. The tensile strength index of the samples also increased in all 3 concentrations after treatment, however after aging, the tensile strength index of the samples decreased compared with the previous phase. The highest tensile strength after treatment was observed in samples with 2% treatment at 28.2 and after aging 26. 3 Nm/g per meter.}, keywords = {Cellulose Nanofibers,historical paper relics,Optical Features,mechanical strength features}, title_fa = {تأثیر نانوالیاف سلولز بر خواص نوری و مکانیکی آثار کاغذی تاریخی}, abstract_fa = {هدف این پژوهش، ارزیابی تأثیر ماده نانوالیاف سلولز و استفاده از آن به‌عنوان استحکام‌بخش جهت بازگرداندن مقاومت کششی و استحکام به آثار کاغذی تاریخی است. روش انجام پژوهش تحلیلی- مقایسه­ای و شیوه گردآوری داده­ها از طریق آزمایش­های مرتبط با موضوع پژوهش همچون pH سنجی، رنگ­سنجی و اندازه­گیری مقاومت کششی نمونه­ها بوده است. در این پژوهش تیمار نانو الیاف سلولز با درصدهای وزنی 5/0، 1 و 2 درصد، به­صورت سوسپانسیون با آب تهیه شد و جهت استحکام‌بخشی نمونه‌های کاغذ، مورد استفاده قرار گرفت. تیمار حاصل روی نمونه­های کاغذی سه بار به­وسیله اسپری دستی به مقدار 3 میلی­­لیتر اسپری شد و سپس نمونه­های تیمار شده بر اساس استاندارد D776-92 ASTM، در دمای 105 درجه سانتی‌گراد به مدت 144 ساعت تحت کهنه­سازی حرارتی قرار گرفتند. در مرحله بعد تغییرات pH، رنگ و مقاومت کششی نمونه­ها مورد بررسی قرار گرفت. نتایج نشان داد که مقدار pH نمونه­ها پس از تیمار در محدوده 98/6 تا 17/7 و بعد از عمل کهنه­سازی نیز pH نمونه­ها در محدوده نزدیک به قلیایی 85/6 تا 11/7 قرار گرفته است. شاخص مقاومت کششی نمونه­ها نیز در هر 3 غلظت پس از تیمار افزایش پیدا کرده است اما پس از کهنه­سازی شاخص مقاومت کششی نمونه‌ها نسبت به مرحله قبل کاهش‌یافته است. بیشترین مقدار مقاومت کششی در مرحله بعد از تیمار مربوط به نمونه­های با تیمار 2 درصد به‌اندازه 2/28 و پس از کهنه­سازی به‌اندازه 3/26 نیوتن متر بر گرم است.}, keywords_fa = {نانوالیاف سلولز,آثار کاغذی تاریخی,خواص نوری,خواص مکانیکی}, url = {https://www.ijwp.ir/article_44487.html}, eprint = {https://www.ijwp.ir/article_44487_f39137c1509df651c17c5d1e47f4bae8.pdf} }